Here is a great overview on ALD for coating complex 3D compnents for optics from LASEROPTIK, Germany (LINK).
Laseroptik offers ALD coatings ranging from UV to IR.
Atomic Layer Deposition for Coating of Complex 3D Optics - From theory to practice
Abstract: Atomic Layer Deposition (ALD) is a chemical vapor coating technique that
has recently been adapted for precision laser optics to perform highly
conformal multilayer coatings on complex 3D substrates like hemispheres,
axicons or multi-sided prisms. In our brief report, we explain some ALD
fundamentals and describe the way from idea and single-layer films to
simple AR (anti-reflection) coatings and even more ambitious designs,
like non-polarizing beam splitters, performed on complex optical
substrates.
The article contains a new nice graphical representation of CVD vs. ALD process description that I have not seen before - reminds me of winter vs an April typ of weather changing all thee time between winter and summer, rain, snow and sunshine.
CVD vs- ALD (Screen sump, http://onlinelibrary.wiley.com/doi/10.1002/opph.201700013/epdf)
LASEROPTIK is a German manufacturer of high power laser optics and coatings from VUV to IR, using PVD methods like e-beam evaporation, ion assisted deposition, magnetron sputtering, ion beam sputtering and recently the chemical vapor method of atomic layer deposition. LASEROPTIK runs more than thirty coating machines and processes about 150,000 optics per year, from needle head size to laser mirrors of up to two meters in length. The company was founded in 1984 by Dr. Johannes Ebert as a spin-off from Hanover University. Main customers are laser manufacturers from industry, medicine and scientific research.
%20(1).png)


Your article was very impressive; I really appreciate the research you’ve done and that helps make your article rich. Overall you’ve done great work.
ReplyDeletealuminum mirror quotation
Your blog is very useful and provide tremendous facts. It is going to change the way one think by a sharp angle. I wonder if you write on gadgets also. Keep up the good work ahead.
ReplyDeleteoptical black coating
I must thank you for posting this blog because the topic is in very demand today and everyone wants to read about it. You have given us an appropriate option.
ReplyDeletegermanium wafer
You always write fabulous. This is third time I am reading any of your blog and again finding it inspirational one. And I am sure this number is going to be increased.
ReplyDeleteflat optics
I really appreciate your research work. Hope to read more articles on your blog site. Keep it up dear.
ReplyDeleteoptical flat